Nanoindentation is a technique for measuring the mechanical properties, such as elastic modulus and hardness, of surfaces on a very small scale. The method is fast and effective, and it can be used on either very small samples or specific locations within a larger object. Nanoindentation provides precise information on the properties of various sample types, including thin films, polymers, biological materials, and electronic components.

What is nanoindentation?
Nanoindentation is a process by which mechanical properties, such as elastic modulus and hardness, are measured. It can also provide information on a material's stiffness, fracture toughness, delamination, tensile strength, and stress relaxation. Nanoindentation can be used to monitor these properties on a wide range of sample sizes, including very small components and specific areas of larger samples. The method is widely used in mechanical engineering and product development.
Nanoindentation covers several different kinds of methods: quasi-static, dynamic, and continuous stiffness measurements. The traditional testing method consists of a simple quasi-static load indentation. Load and depth of indentation are measured and the sample material's mechanical properties are calculated. Dynamic nanoindentation uses oscillating load variation to extract the properties of the tested material. Continuous stiffness measurement (CSM) is a combination of static and dynamic loads during indentation. This allows the measurement of depth-dependent properties quickly and efficiently.
How does nanoindentation work?
In nanoindentation, a very small probe tip made of a hard material, usually a diamond, is used to indent the surface of a sample. The system measures the load applied to the tip as well as the depth of indentation during the process. Over time, the force applied to the probe and the distance it moves to the surface are measured.

Nanoindentation and atomic force microscopy
Atomic force microscopes can conduct similar analyses to nanoindentation measurements, as long as the sample material is softer than the AFM tip. The probe is traced over the surface and its positional data is recorded along with the topographic measurements of the sample surface. This can then be used to produce an image of the surface on a tiny scale, allowing it to be further analyzed. Most modern nanoindentation instruments can be directly coupled with AFM analysis to reach the most efficient and precise measurements.
Applications
Nanoindentation is used in several fields of science and engineering to characterize materials including electronics, packaging materials, biological samples, construction materials, and polymers. More precisely, nanoindentation is typically used for thin films, alloys, soft tissues, coatings, and composites. The method finds particular use in modern technology, where components are becoming increasingly smaller. Nanoindentation is an excellent way to analyze these structures and provides valuable information on their physical properties.
Sample requirements and preparation
In principle, nanoindentation requires no sample preparation. However, loose samples and objects can generally not be placed in the nanoindenter. If the sample is loose, it can be super-glued to an AFM specimen disk, glass slide, or wafer. The roughness of the sample surface affects the measured mechanical properties. For this reason, the roughness of the sample surface should be large enough compared to the area of the tip.
Limitations of nanoindentation
Depending on the material characteristics, “pile-up” or “sink-in” of the sample material can cause problems in indentation depth calculations. For this reason, measurements on either very soft or very rough surfaces can be challenging or even impossible.
Need an analysis?
Measurlabs offers high-quality laboratory analyses with nanoindentation. Whether it’s just a dozen of samples or a large series, we offer competitive pricing and deliver reliable results quickly. Our experts are just a message away, ready to guide you from method selection to result interpretation with clarity and care. Contact us through the form below to get a quote and start the discussion.
Suitable sample matrices
- Polymers
- Thin films
- Alloys
- Biological samples
- Microelectronics
Ideal uses of nanoindentation
- Analyzing specific areas of a sample
- Determination of local mechanical properties
- Testing very small samples
- Probing soft tissue samples
- Examining thin film materials
- Thin film adhesion
- Modulus mapping
- Failure analysis for e.g. coatings
- Structural compliance testing
Ask for an offer
Fill in the form, and we'll reply in one business day.
Have questions or need help? Email us at [email protected] or call our sales team.
Frequently asked questions
Nanoindentation is used for analyzing the mechanical properties of surfaces on a very small scale. Examples of the properties studied with nanoindentation are hardness, elastic modulus, stiffness, fracture toughness, delamination, tensile strength, and stress relaxation.
Analyses of very soft or rough surfaces can be challenging or even impossible due to "pile up" or "sink in" of the material.
Nanoindentation can be used for analyzing polymers, thin films, alloys, microelectronics, and biological samples.